Repair method for corroded end covers, rebuilding with epoxy compound, and protective coating application.

Done by the crew on board, during voyage.Super Metal Filler Compound
Step-by-step illustration: Heat exchanger end plate - Repair
Illustrations from the SepcoTech epoxy instruction handbook. Includes AI generated images.

Step by step

  1. Sand down the existing epoxy to the reference level according to liner requirements.

  2. Create a Casting Mould reference to required liner dimension (hole size).

  3. Apply Release Agent on the Casting Mould.

  4. Apply Super Metal Filler on the Casting Mould and in the hole.

  5. Fixate the Casting Mould in correct position.

  6. Await curing time (allow 12 hrs).

  7. Remove the Casting Mould (pull it out). Then you have the exact copy of the mould.