Deep pitting across the hull plating, rebuilt with epoxy filler and recoated in three steps. Accepted by the attending ABS surveyor: no hot work, no steel renewal, no tanks to gas free.
Prefer to talk? Call (+45) 6916 2400 or email tech@sepcotech.com
Before
AfterHigh-pressure water jetting takes off the corrosion and loose scale from the pitted areas.
Where the bottom of the pits is still rusty after jetting, the Rotating Blaster Duo cleans it back to bright steel on an ordinary drill, before Super Metal Filler goes in.

An epoxy wetting layer goes on first. Then Super Metal Filler Compound rebuilds the pits and is faired back to the plating profile.



After cure the areas are prepared again and the vessel's own hull coating system goes back on.
This case as a four-page PDF, ready to print or forward to the technical superintendent.
Before
AfterContainer vesselLeaking, corroded pipes inside the ballast tanks, sealed in place by the crew.
See the repair
Before
AfterSupertankerCracked GRE pipes and a displaced coupling, bonded and sealed inside the ballast tanks.
See the repair
Before
AfterSteel and GRE pipesBlasted, then rebuilt with four coats of Super Guard and three layers of Super Wrap.
See the repair
Before
AfterSea chestCleaned with fresh water and coated straight away, back in service three days later.
See the repairTell us the dimensions, whether the surface is wet or dry, and the operating temperature and pressure. We normally reply within one business day.
No obligation. If another approach suits the damage better, we will say so.