Skip to the content
Case · Steel and GRE pipes

A corroded pipe rebuilt with epoxy and wrap.

The whole repair in five steps: blast, then coat and wrap, layer by layer, until there are four coats of Super Guard and three layers of Super Wrap. Works on steel and GRE, up to 180 °C.

Prefer to talk? Call (+45) 6916 2400 or email tech@sepcotech.com

Before: Corroded pipe, before preparationBefore
Corroded pipe, before preparation
After: Built up with Super Guard Coating Blue, White and Super WrapAfter
Built up with Super Guard Coating Blue, White and Super Wrap
Pipes
Steel and GRE
Service
Up to 180 °C, also submerged
Build-up
4 coats, 3 wraps
Per coat
500 to 700 µm wet
Blast profile
50 to 75 µm
Hot work
None
The repair

Step by step.

  1. Corroded pipe repaired with epoxy and Super Wrap – step 1, Inspect and clean

    Inspect and clean

    Check the pipe for corrosion, scale, old coating and oil, and mark out the repair area at least 10 cm beyond the damage. Degrease with Bio Cleaner and let it dry.

    Bio Cleaner #10254
  2. Corroded pipe repaired with epoxy and Super Wrap – step 2, Blast to near-white metal (photo 1 of 2)Corroded pipe repaired with epoxy and Super Wrap – step 2, Blast to near-white metal (photo 2 of 2)

    Blast to near-white metal

    Move the Rotating Blaster Duo steadily along the section, to near-white metal with a 50 to 75 µm profile for the epoxy to grip.

  3. Corroded pipe repaired with epoxy and Super Wrap – step 3, Coat 1: Super Guard Coating Blue (photo 1 of 2)Corroded pipe repaired with epoxy and Super Wrap – step 3, Coat 1: Super Guard Coating Blue (photo 2 of 2)

    Coat 1: Super Guard Coating Blue

    Apply straight from the cartridge or mix onto a board. Brush or roll it on evenly, 500 to 700 µm wet, with no dry spots or air pockets.

  4. Corroded pipe repaired with epoxy and Super Wrap – step 4, Wrap while the coat is tacky (photo 1 of 2)Corroded pipe repaired with epoxy and Super Wrap – step 4, Wrap while the coat is tacky (photo 2 of 2)

    Wrap while the coat is tacky

    Wrap Super Wrap from one end with constant tension and 50% overlap while the coat is still wet and tacky. Let it semi-cure.

  5. Corroded pipe repaired with epoxy and Super Wrap – step 5, Coat 2 in white, wrap again, build up (photo 1 of 3)Corroded pipe repaired with epoxy and Super Wrap – step 5, Coat 2 in white, wrap again, build up (photo 2 of 3)Corroded pipe repaired with epoxy and Super Wrap – step 5, Coat 2 in white, wrap again, build up (photo 3 of 3)

    Coat 2 in white, wrap again, build up

    Coat the semi-cured wrap with Super Guard Coating White and wrap again the same way. Repeat until there are four coats and three wraps: the alternating colours show every coat is covered.

Get in touch

Describe the damage.
We'll specify the repair.

Tell us the dimensions, whether the surface is wet or dry, and the operating temperature and pressure. We normally reply within one business day.

Request a quote or repair advice

No obligation. If another approach suits the damage better, we will say so.

Or email tech@sepcotech.com · Tel. (+45) 6916 2400

Call Get a quote in 1 day